產品說明 Description
該漆以羥基丙烯酸樹脂為基料,以HDI-縮二尿為乙組份,漆膜有良好的物理機械性能,優異的防腐性能,耐濕熱、耐鹽霧、保光、保色生及耐候性突出。
It has been developed based on hydroxyl acrylic resin, and using HDI-biuret as Component II. Its film has good physical and mechanical properties, and excellent corrosion protection, and resistance to hot and humid and salt mist, outstanding color and light protection and weatherability.
設計用途 Use
用于船舶、橋梁、鋼結構作防腐面漆。
Corrosion protection for ships, bridges and steel structures.
物理參數 Physical Parameter
顏 色: 各色
光 澤: 有光
理論涂布率: 240g/m2(以干膜75μm計,不含損耗)
比 重: 約1.26~1.27
干燥時間: 23±2℃:表干≤0.5 h, 實干≤24h
閃 點: 27℃
貯 存 期: 6個月
Color: Various Colors
Gloss: Glossy
Theoretical Spreading Rate: 240g/m2 (dry film75μm, excluding loss)
Specific Gravity: Approx. 1.26~1.27
Drying Time: 23±2℃:Surface Dry≤0.5 h; Hard Dry≤24h
Fully Cured Time: 23±2℃:7 days
Flash Point:27℃
Storage Life: 6 months
施工說明 Description of Application
混合配比: 甲組份:乙組份=20:4
熟化時間: 23±2℃:20min
適 用 期: 23±2℃:6 h
施工方法: 高壓無氣噴涂 有氣噴涂 手工刷涂、輥涂
稀 釋 劑: 丙烯酸聚氨酯涂料稀釋劑
Mixture Ratio: Component I:Component II=20:4
Maturing Time: 23±2℃:20min
Pot Life: 23±2℃:6 h
Application Method: High Pressure Airless Spraying, Air Spraying, Manual Brush Coating and Roller Painting.
Thinner: Acrylic Polyurethane Paint Thinner
高壓無氣噴涂 |
有氣噴涂 |
手工刷涂、輥涂 |
10% |
20% |
5% |
0.4-0.5mm |
2.0-2.5mm |
— |
15-20MPa |
0.3-0.4 Mpa |
— |
最大稀釋量Max. Usage of Thinner
噴 孔Spray Orifice
噴出壓力Pressure When Spraying
工具清洗 丙烯酸聚氨酯涂料稀釋劑
Tool Cleaning: Acrylic Polyurethane Paint Thinner
漆膜厚度 濕膜:170μm 干膜75μm
Film Thickness: Wet Film: 170μm; Dry Film: 75μm
涂裝間隔 23±2℃:最短2 h,最長7d
Painting Interval: 23±2℃: Min. 2 h; Max.7d
表面處理 Surface Treatment
如前道漆面已經污染,應用適當的方法除去油脂、灰塵,也可用本漆稀釋劑擦洗。
if the preceding coating has been contaminated, appropriated methods should be used to remove grease and dust. Also, the thinner for this paint can be used for cleaning.
施工條件 Application Conditions
氣溫5℃~35℃,相對濕度小于85%,被涂物表面溫度應高于露點3℃以上,在雨、霧、雪和較大灰塵條件下不可施工。
The best coating temperature is 0-35℃ and relative humidity should be less than 85%. Application should be stopped in raining, foggy, snowing weathers and dusty circumstance.
前道配套涂料 環氧富鋅底漆、環氧云鐵防銹漆、無機富鋅底漆
Preceding Coats: Epoxy Zinc-rich Primer, Epoxy Micaceous Iron Anti-rust Paint, Inorganic Zinc-rich Primer
保養期 Maintaining Period
(23±2℃)7 d以上
More than 7 days at 23±2℃.
包裝規格 Packing Specification
甲組份20升容器裝20公斤,乙組份3.4升容器裝4公斤 。
Component I: 20L Container, 20kg; Component II: 3.4L Container, 4kg
備注 Notes
可根據使用目的及部位修改漆膜厚度,但這會相應改變涂布率和干燥時間。
The above index of dry and wet film thickness is under high pressure airless spraying.
All data in this description is obtained in laboratory and slight variation may occur during actual use.
The above specification and description are subject to the change without notice.
注意事項 Attentions
● 若前道涂料涂裝時間過久,涂后道時應用水砂紙打毛,清除掉表面灰塵污物后再涂漆以保證層間附著力。
● 施工所用工具應清潔干燥,涂料不得混入水份及其它雜質,涂料現配現用,須8小時內用完。
● 漆膜未完全干燥固化之前,應采取保護措施,避免受到雨水或其它液體的沖洗和踐踏。
● 涂料存放于溫度較低通風干燥處,遠離熱源,避免日光直射,并隔絕火種。
● If the preceding paint has been coated for long time, it should be roughening by waterproof abrasive paper before subsequent coating. Dust and dirt should be removed from the surface first to guarantee the adhesive forces between coatings.
● All tools should be cleaned and dried. No water or other impurities are allowed to mix in the paint. The paint should be used up within 8 hours.
● Protection should be provided for the coating to prevent from damage caused by rain or other liquids before it is completely cured.
● This product should be stored in cool, dry place with good ventilation. Keep it away from heat. Avoid direct sun exposure. Completely cut off fire source.
安全 Safety
避免長期吸入溶劑蒸汽或漆霧,皮膚、眼睛不得接觸本品,在狹窄或空氣不流通處施工,必須提供強力通風,施工時應配防護用具。
To avoid the long-term inhalation of solvent vapor or paint mists. To avoid contacts with skin and eyes. Forced ventilation must be provided when applying paints in confined space or stagnant air. Protective appliance is required during application.
附注 Notes
上述的干濕膜厚度都是指高壓無氣噴涂時的指標;
本說明有關數據是在實驗室取得,實際產品可能與之略有不同;
以上數據如有改變,以本公司最新說明書為準,恕不另行通知。
The above index of dry and wet film thickness is under high pressure airless spraying.
All data in this description is obtained in laboratory and slight variation may occur during actual use.
The above specification and description are subject to the change without notice.